DATA SHEET ON FATIGUE PROPERTIES OF EXTRUDED AZ61(Mg-6Al-1Zn) AND AZ31(Mg-3Al-1Zn) MAGNESIUM ALLOYS
1 of 20
DATA SHEET ON LONG-TERM, HIGH TEMPERATURE LOW-CYCLE FATIGUE PROPERTIES OF NCF800H (21Cr-32Ni-Ti-Al) CORROSION-RESISTING AND HEAT-RESISTING ALLOY PLATE
2 of 20
DATA SHEET ON FATIGUE PROPERTIES OF NON-LOAD-CARRYING CRUCIFORM WELDED JOINTS OF SM490B ROLLED STEEL FOR WELDED STRUCTURE - Effect of Plate Thickness (Part 3, Thickness 80 mm) -
3 of 20
DATA SHEET ON GIGA-CYCLE FATIGUE PROPERTIES OF Ti-6Al-4V ELI (1100MPa CLASS) TITANIUM ALLOY
4 of 20
DATA SHEET ON ULTRASONIC FATIGUE PROPERTIES OF SCM440(0.40C-1Cr-0.2Mo) STEEL FOR MACHINE STRUCTURAL USE
5 of 20
DATA SHEET ON GIGA-CYCLE FATIGUE PROPERTIES OF Ti-6Al-4V ELI (900MPa CLASS) TITANIUM ALLOY
6 of 20
DATA SHEET ON GIGA-CYCLE FATIGUE PROPERTIES OF SCM440(0.40C-1Cr-0.2Mo) STEEL FOR MACHINE STRUCTURAL USE
7 of 20
DATA SHEET ON FATIGUE PROPERTIES OF Ti-6Al-4V ELI (1100MPa CLASS) TITANIUM ALLOY
8 of 20
DATA SHEET ON ULTRASONIC FATIGUE PROPERTIES OF S40C(0.40C) CARBON STEEL FOR MACHINE STRUCTURAL USE
9 of 20
DATA SHEET ON FATIGUE PROPERTIES OF Ti-6Al-4V ELI (900MPa CLASS) TITANIUM ALLOY
10 of 20
DATA SHEET ON LONG-TERM, HIGH TEMPERATURE LOW-CYCLE FATIGUE PROPERTIES OF SUS310S (25Cr-20Ni) HOT ROLLED STAINLESS STEEL PLATE
11 of 20
DATA SHEET ON FATIGUE PROPERTIES OF NON-LOAD-CARRYING CRUCIFORM WELDED JOINTS OF SM490B ROLLED STEEL FOR WELDED STRUCTURE - Effect of Plate Thickness (Part 2, Thickness 160mm) -
12 of 20
DATA SHEET ON GIGA-CYCLE FATIGUE PROPERTIES OF Ti-6Al-4V (1100MPa CLASS) TITANIUM ALLOY
13 of 20
DATA SHEET ON GIGA-CYCLE FATIGUE PROPERTIES OF S40C (0.40C) CARBON STEEL FOR MACHINE STRUCTURAL USE
14 of 20
DATA SHEET ON FATIGUE PROPERTIES OF NON-LOAD-CARRYING CRUCIFORM WELDED JOINTS OF SM490B ROLLED STEEL FOR WELDED STRUCTURE - Effect of Plate Thickness (Part 1, Thickness 9 mm) -
15 of 20
DATA SHEET ON FATIGUE PROPERTIES OF PURE TITANIUM
16 of 20
DATA SHEET ON LONG-TERM, HIGH TEMPERATURE LOW-CYCLE FATIGUE PROPERTIES OF SCMV 4(2.25Cr-1Mo) STEEL PLATE FOR BOILERS AND PRESSURE VESSELS
17 of 20
DATA SHEET ON ULTRASONIC FATIGUE PROPERTIES OF SUP7 (2.0Si-0.8Mn) STEEL FOR SPRINGS
18 of 20
DATA SHEET ON GIGA-CYCLE FATIGUE PROPERTIES OF Ti-6Al-4V (900MPa CLASS) TITANIUM ALLOY
19 of 20
DATA SHEET ON FATIGUE PROPERTIES OF NON-LOAD-CARRYING CRUCIFORM WELDED JOINTS OF SM490B ROLLED STEEL FOR WELDED STRUCTURE - Effect of Residual Stress -