Interfacial Strength Evaluation Between Sulfur-Segregated Al2O3 and Ni–Al Single Crystal Alloy Using Nanoindentation
Proceedings
Creator
Chihiro Tabata
;
Toshio Osada
;
Takahito Ohmura
; Tadaharu Yokokawa ;
Kyoko Kawagishi
; Shinsuke Suzuki
Keyword
nanoindentation
,
oxidation
,
sulfur segregation
,
interfacial strength
,
Ni-base single crystal alloy
Date published
2024-08-21
Updated at
2025-08-21 08:30:48 +0900
Keyword
Ni-base single crystal alloy
(1)
interfacial strength
(1)
nanoindentation
(1)
oxidation
(1)
sulfur segregation
(1)