Keyword: Ni-Co-based superalloy

1 record found.

3Dcrack video withoutGB slow.mov
Three-dimensional high-resolution crystallographic observation of the entire volume of microstructurally small fatigue cracks in Ni-Co based superalloy
Journal article
Creator
Hideaki Nishikawa (author) (Search by this author)
ORCID SAMURAI ;
Yoshiyuki Furuya (author) (Search by this author)
ORCID SAMURAI ;
Toshio Osada (author) (Search by this author)
ORCID SAMURAI ;
Kyoko Kawagishi (author) (Search by this author)
ORCID SAMURAI ;
Toru Hara (author) (Search by this author)
ORCID SAMURAI
Keyword
Small fatigue crack, Crystal orientation, 3D observation, PFIB-SEM, Ni-Co-based superalloy
Date published
2022-09-05
Updated at