説明:
(abstract)An emerging motor type, the variable flux permanent magnet (VFPM) motor, has created a demand for permanent magnets with a new set of properties. These magnets must exhibit easily tunable magnetization, demanding for moderate coercivity values, low magnetizing fields, and first-order reversal curves (FORCs) with high flatness. In this work, we report that the doping of Sm and La in Nd-Fe-B-based hot-deformed magnet, followed by the Nd-Cu diffusion process, resulted in desirable magnetic properties, such as, a moderate coercivity (µ0Hc) of 0.55 T, a low magnetizing field (µ0Hmag) of 0.94 T and a high FORC flatness of 0.96, while maintaining a high remanence (µ0Mr) of 1.3 T. The FORC flatness achieved in this work is the highest and the comprehensive properties are superior to the previously reported Nd-Fe-B magnets for VFPM motors. Microscopic investigations revealed that the high flatness achieved in this hot-deformed magnet is attributed to the formation of Fe-lean thick intergranular phases realized by Nd-Cu grain boundary diffusion. The overall combination of the magnetic properties for the diffusion processed (Nd,Sm,La)-Fe-B magnet is excellent, in comparison with a commercially available Sm2Co17-type magnet, showing the promise of the former for use in VFPM motors.
権利情報:
キーワード: Nd-Fe-B magnet, Coercivity First-order reversal curves Variable-flux permanent magnet motors
刊行年月日: 2024-09-12
出版者: Elsvier
掲載誌:
研究助成金:
原稿種別: 査読前原稿 (Author's original)
MDR DOI: https://doi.org/10.48505/nims.5124
公開URL: https://doi.org/10.1016/j.actamat.2024.120387
関連資料:
その他の識別子:
連絡先:
更新時刻: 2024-12-10 16:55:46 +0900
MDRでの公開時刻: 2024-12-10 16:55:46 +0900
| ファイル名 | サイズ | |||
|---|---|---|---|---|
| ファイル名 |
Manuscript.docx
(サムネイル)
application/vnd.openxmlformats-officedocument.wordprocessingml.document |
サイズ | 7.56MB | 詳細 |