キーワード: Nickel-based superalloy

1 件のレコードが見つかりました。 1件目から1件目まで表示します。

別刷.pdf
Creep data sheet for Nickel-based 19Cr-18Fe-3Mo-5Nb-Ti-Al superalloy
ジャーナル論文
著者
Kota Sawada (author) (この著者で検索)
National Institute for Materials Science Research Center for Structural Materials/Materials Evaluation Field/Creep Property Group
ORCID SAMURAI ;
Yasushi Taniuchi (author) (この著者で検索)
National Institute for Materials Science Research Network and Facility Services Division/Materials Data Platform/Creep Data Unit
ORCID SAMURAI ;
Kaoru Sekido (author) (この著者で検索)
National Institute for Materials Science Research Network and Facility Services Division/Materials Data Platform/Creep Data Unit
ORCID SAMURAI ;
Takehiro Nojima (author) (この著者で検索)
National Institute for Materials Science Research Network and Facility Services Division/Materials Data Platform/Creep Data Unit
ORCID SAMURAI ;
Tomotaka Hatakeyama (author) (この著者で検索)
National Institute for Materials Science Research Center for Structural Materials/Materials Evaluation Field/Creep Property Group
ORCID SAMURAI ;
Kazuhiro Kimura (author) (この著者で検索)
National Institute for Materials Science Research Center for Structural Materials
ORCID SAMURAI
キーワード
Nickel-based superalloy, 100,000h creep rupture strength, heat-to-heat variation
刊行年月日
2024-12-31
更新時刻
2024-12-05 12:47:31 +0900