110_TETSU-2024-069.pdf
Origin of Serrated Markings on the Hydrogen Related Quasi-cleavage Fracture in Low-carbon Steel with Ferrite Microstructure
論文
著者
Kazuho Okada SAMURAI ORCID ; Akinobu Shibata SAMURAI ORCID ; Hisashi Matsumiya ORCID ; Nobuhiro Tsuji ORCID
キーワード
hydrogen embrittlement, ferritic steel, quasi-cleavage fracture, transmission electron microscopy (TEM), focused ion beam (FIB), three-dimensional morphology
刊行年月日
2024-09-01
更新時刻
2024-09-03 12:30:16 +0900

キーワード
  • ferritic steel (1)
  • focused ion beam (FIB) (1)
  • hydrogen embrittlement (1)
  • quasi-cleavage fracture (1)
  • three-dimensional morphology (1)
  • transmission electron microscopy (TEM) (1)
  • <
  • 1
  • >

国立研究開発法人 物質・材料研究機構

技術開発・共用部門
材料データプラットフォーム

お問い合わせ

  • 利用規約
  • プライバシーポリシー
  • Data Platform DICE
  • Researchers Directory SAMURAI
  • NIMS Digital Library
© National Institute for Materials Science. Datasets are available under licenses specified on their pages.