MDR
  • About
  • Help
  • Contact
  • 表示言語の変更
    日本語 English
  1. Home
  2. Article and Dataset

  • Article(1)
  • Laser powder bed fusion (1)
  • Nickel-base superalloy (1)
  • Part-scale finite element thermal analysis (1)
  • Temperature control (1)
  • Time per layer (1)
(more)
  • Creative Commons BY-NC-ND Attribution-NonCommercial-NoDerivs 4.0 International (1)
  • application/pdf (1)
Keyword: Nickel-base superalloy
Reset all filters

1 record found.

1-s2.0-S1526612524009071-main.pdf
Controlling heat accumulation through changing time per layer in laser powder bed fusion of nickel-based superalloy
Article
Creator
Masahiro Kusano SAMURAI ORCID ; Makoto Watanabe SAMURAI ORCID
Keyword
Temperature control, Laser powder bed fusion, Part-scale finite element thermal analysis, Time per layer, Nickel-base superalloy
Date published
2024-09-12
Updated at
2024-11-21 16:30:41 +0900

Keyword
  • Laser powder bed fusion (1)
  • Nickel-base superalloy (1)
  • Part-scale finite element thermal analysis (1)
  • Temperature control (1)
  • Time per layer (1)
RDE metadata def
RDE invoice schema
  • <
  • 1
  • >

National Institute for Materials Science

Research Network and Facility Services Division (RNFS)
Materials Data Platform

Contact

  • Terms of use
  • Privacy Policy
  • Researchers Directory SAMURAI
  • NIMS Digital Library
  • Data Platform DICE
© National Institute for Materials Science. Datasets are available under licenses specified on their pages.