3 records found.
Effect of Solution Heat Treatment on Dendritic Segregation and Creep Strength of Ni-Base Single Crystal Superalloy TMS-238
Article
Creator
Tadaharu Yokokawa
;
Toshio Osada
;
Chihiro Tabata
; Takuma Kohata ;
Yuji Takata
;
Michinari Yuyama
;
Kyoko Kawagishi
Keyword
Ni-base superalloy
,
single crystal
,
solution heat treatment
,
segregation
,
high-temperature creep strength
Date published
2024-11-01
Updated at
2024-12-25 16:31:02 +0900
Improvement of Oxidation Resistance for Ni-Base Single Crystal Superalloy TMS-238 by Suppression of Sb Segregation at Oxide/Substrate Interface Using CaO
Article
Creator
Hirotoshi Maezawa ;
Chihiro Tabata
;
Yuji Takata
;
Jun Uzuhashi
;
Tadakatsu Ohkubo
;
Tadaharu Yokokawa
; Hiroshi Harada ;
Kyoko Kawagishi
; Shinsuke Suzuki
Keyword
Ni-base superalloy
Date published
2023-11-07
Updated at
2024-11-07 16:30:28 +0900
Effect of Ca Addition on the Oxidation Resistance of Ni–Al Alloy
Article
Creator
Chihiro Tabata
;
Kyoko Kawagishi
;
Tadaharu Yokokawa
;
Jun Uzuhashi
;
Tadakatsu Ohkubo
; Hiroshi Harada ; Shinsuke Suzuki
Keyword
oxidation resistance
,
sulfur segregation
,
Ni-base superalloy
Date published
2022-12-24
Updated at
2024-01-05 22:12:13 +0900
Keyword
Ni-base superalloy
(3)
high-temperature creep strength
(1)
oxidation resistance
(1)
segregation
(1)
single crystal
(1)
solution heat treatment
(1)
sulfur segregation
(1)
RDE metadata def
RDE invoice schema
<
1
>