Resource type: journal_article Keyword: nanoindentation

8 records found.

Marked-up manuscript_rev3.docx
Grain size dependence of intergranular lattice strain generated by plastic deformation in ferritic steel
Article
Creator
Yo Tomota ORCID ; Hongxing Li ; Noriyuki Tsuchida ; Wu Gong ORCID ; Stefanus Harjo ORCID ; Takahito Ohmura SAMURAI ORCID
Keyword
nanoindentation
Date published
2025-09-22
Updated at
2025-12-12 08:30:20 +0900

1-s2.0-S2589152925000791-main.pdf
Enhanced deformability of TiC in Mo-Ti-C ternary system by off-stoichiometry
Article
Creator
Shuntaro Ida ORCID ; Eri Nakagawa SAMURAI ORCID ; Viola Paul ; Takahito Ohmura SAMURAI ORCID ; Kyosuke Yoshimi ORCID
Keyword
nanoindentation
Date published
2025-04-17
Updated at
2025-12-12 08:30:15 +0900

adom202203139-sup-0001-suppmat.pdf
Bright Lanthanide III Triboluminescence despite Low Photoluminescence, and Dual Triboluminescence and Mechano‐Responsive Photoluminescence
Article
Creator
Yuichi Hirai SAMURAI ORCID ; Stann Van Baaren ; Takahito Ohmura SAMURAI ORCID ; Takayuki Nakanishi SAMURAI ORCID ; Takashi Takeda SAMURAI ORCID ; Yuichi Kitagawa ; Yasuchika Hasegawa ; Rémi Métivier ; Clémence Allain
Keyword
stimuli responsive mateirlas, luminescence, nanoindentation, stress sensor, solid mechanics
Date published
2023-02-08
Updated at
2024-07-04 16:30:29 +0900

ando_ISIJINT2021.pdf
Analysis of Nano-hardness Distribution Near the Ferrite-martensite Interface in a Dual Phase Steel with Factorization of Its Scattering Behavior
Article
Creator
Reon Ando ; Takashi Matsuno ; Tomoko Matsuda ; Norio Yamashita ; Hideo Yokota ; Kenta Goto ORCID ; Ikumu Watanabe SAMURAI ORCID
Keyword
dual phase steel, grains and interfaces, scattering, nanoindentation, serial sectioning
Date published
2021-01-15
Updated at
2024-01-05 22:13:56 +0900