Analysis of Nano-hardness Distribution Near the Ferrite-martensite Interface in a Dual Phase Steel with Factorization of Its Scattering Behavior
Journal article
Creator
Reon Ando (author) (Search by this author)
;
Takashi Matsuno (author) (Search by this author)
;
Tomoko Matsuda (author) (Search by this author)
;
Norio Yamashita (author) (Search by this author)
;
Hideo Yokota (author) (Search by this author)
;
Kenta Goto (author) (Search by this author)
National Institute for Materials Science
ORCID ;
Ikumu Watanabe (author) (Search by this author)
ORCID SAMURAI
Keyword
dual phase steel, grains and interfaces, scattering, nanoindentation, serial sectioning
Date published
2021-01-15