2024_Ohno_EPRI 2024_Homogenization During Solution Heat Treatment of Ni-Base Single-Crystal Superalloy TMS-238.pdf
Homogenization during solution heat treatment of Ni-base single-crystal superallloy TMS-238
プレゼンテーション
著者
Naoki Ohno (author) (この著者で検索)
National Institute for Materials Science Research Center for Structural Materials/Materials Manufacturing Field/High Temperature Materials Group
;
Toshio Osada (author) (この著者で検索)
National Institute for Materials Science Research Center for Structural Materials/Materials Manufacturing Field/High-Reliability Heat-Resistant Materials Group
ORCID SAMURAI ;
Chihiro Tabata (author) (この著者で検索)
National Institute for Materials Science Research Center for Structural Materials/Materials Manufacturing Field/High Temperature Materials Group
ORCID SAMURAI ;
Tadaharu Yokokawa (author) (この著者で検索)
National Institute for Materials Science Human Resources Division
ORCID SAMURAI ;
Ayako Ikeda (author) (この著者で検索)
National Institute for Materials Science Research Center for Structural Materials/Materials Manufacturing Field/High Temperature Materials Group
ORCID SAMURAI ;
Kyoko Kawagishi (author) (この著者で検索)
National Institute for Materials Science Research Center for Structural Materials/Materials Manufacturing Field/High Temperature Materials Group
ORCID SAMURAI ;
Shinsuke Suzuki (author) (この著者で検索)
Waseda Univeristy
キーワード
apparent diffusion constant, dendritic segregations, homogenization, nickel single crystal superalloys, solution heat treatment
刊行年月日
更新時刻
2025-03-14 16:30:18 +0900