1 record found.
Observation and Numerical Prediction of Concentration Distribution at Cast Coating Interface of Solid Pt, Ir, Re Using Liquid Ni-Based Alloys
Article
Creator
Machiko Ode
; Hisao Esaka ;
Akira Ishida
;
Susumu Takamori
;
Hideyuki Murakami
Keyword
cast-coating
,
Ni-based superalloy
,
solid/liquid interface
,
solidification simulation
Date published
2024-05-01
Updated at
2025-01-09 16:30:58 +0900
Keyword
Ni-based superalloy
(1)
cast-coating
(1)
solid/liquid interface
(1)
solidification simulation
(1)
RDE metadata def
RDE invoice schema
<
1
>