1-s2.0-S0264127525006999-main.pdf
Automated system for high-throughput process-structure-property dataset generation of structural materials: A γ/γ′ superalloy case study
Journal article
Creator
Thomas Hoefler (author) (Search by this author)
ORCID https://orcid.org/0000-0003-0650-179X
SAMURAI NIMS Researchers Directory SAMURAI
ORCID SAMURAI ;
Ayako Ikeda (author) (Search by this author)
ORCID https://orcid.org/0000-0002-1705-9004
SAMURAI NIMS Researchers Directory SAMURAI
ORCID SAMURAI ;
Toshio Osada (author) (Search by this author)
ORCID https://orcid.org/0000-0003-1539-9264
SAMURAI NIMS Researchers Directory SAMURAI
ORCID SAMURAI ;
Toru Hara (author) (Search by this author)
ORCID https://orcid.org/0000-0002-9715-6444
SAMURAI NIMS Researchers Directory SAMURAI
ORCID SAMURAI ;
Kyoko Kawagishi (author) (Search by this author)
ORCID https://orcid.org/0000-0001-7652-9232
SAMURAI NIMS Researchers Directory SAMURAI
ORCID SAMURAI ;
Takahito Ohmura (author) (Search by this author)
ORCID https://orcid.org/0000-0001-7528-566X
SAMURAI NIMS Researchers Directory SAMURAI
ORCID SAMURAI
Keyword
high-throughput method, Nanoindentation, Image analysis, γ/γ' superalloy, Aging heat treatment
Date published
2025-06-20
Updated at
2025-07-01 12:30:19 +0900

Keyword
  • Aging heat treatment (1)
  • Image analysis (1)
  • Nanoindentation (1)
  • high-throughput method (1)
  • γ/γ' superalloy (1)
RDE metadata def
RDE invoice schema
  • <
  • 1
  • >

National Institute for Materials Science

Advanced Engineering and Services Division (AESD)
Materials Data Platform

Contact

  • Terms of use
  • Privacy Policy
  • Researchers Directory SAMURAI
  • NIMS Digital Library
  • Data Platform DICE
© National Institute for Materials Science. Datasets are available under licenses specified on their pages.