@misc{sawada1997a, title = {DATA SHEETS ON THE ELEVATED-TEMPERATURE STRESS RELAXATION PROPERTIES OF 1Cr-0.5Mo-0.25V STEEL AND 12Cr-1Mo-1W-0.3V STEEL BOLTING MATERIALS FOR HIGH TEMPERATURE SERVICE}, author = {SAWADA, Kota, KUSHIMA, Hideaki, NOJIMA, Takehiro, WATANABE, Takashi, SEKIDO, Kaoru, MIYAZAKI, Hideko, HONGO, Hiromichi, TANIUCHI, Yasushi, ABE, Fujio, OHBA, Toshio, KIMURA, Kazuhiro}, publisher = {National Institute for Materials Science}, year = {1997-03-31}, keywords = {} }