# Effect of Pressure on Steam/Supercritical Water Oxidation of 9Cr Steel and 18Cr Steel at 650°C

https://mdr.nims.go.jp/datasets/7c3e271c-7002-4722-a2a9-e180a8711670

## File

- [20267Toda-ISIJInt.pdf](https://mdr.nims.go.jp/filesets/9563e6fb-f5f1-4eab-9cec-a923bf1f20e7/download) ([Detail](https://mdr.nims.go.jp/filesets/9563e6fb-f5f1-4eab-9cec-a923bf1f20e7.md))

## Id

7c3e271c-7002-4722-a2a9-e180a8711670

## Local identifier



## Visibility

open_to_public

## State

published

## Created at

2026-11-15T01:05:23.833481Z

## Updated at

2026-11-16T02:51:45.082516Z

## Published at

2026-11-17T09:29:01.159026Z

## Doi



## First published url

https://doi.org/10.2355/isijinternational.isijint-2026-179

## Date published

2026-11-15

## Recorded date published

2026

## Resource type

journal_article

## Manuscript type

vor

## Collection



## Title

- title: Effect of Pressure on Steam/Supercritical Water Oxidation of 9Cr Steel and
    18Cr Steel at 650°C
  title_type: original
  lang: en

## Description

- description: 9Cr ferritic/martensitic heat-resistant steel and 18Cr austenitic steel
    were exposed for various durations in a pressure vessel to steam (0.5 MPa), subcritical
    water (10.2 MPa), and supercritical water (22.7 MPa) at 650 °C. The pressure dependence
    of the oxidation rate constants of each material was determined from the time
    dependence of specimen weight gain and oxide scale thickness due to oxidation.
    The oxidation rate constants of both steels decreased with increasing pressure.
    In steam, the oxidation rate constant of the 18Cr steel was smaller than that
    of the 9Cr steel. The difference between the two steels decreased with increasing
    pressure, and the oxidation rate constants of the two steels became almost identical
    in supercritical water. These results suggest that, at 650 °C, boilers and pressure
    vessels can be safely operated using higher-pressure steam or supercritical water
    at the same temperature if they are designed based on the oxidation behavior of
    heat-resistant steels in steam at atmospheric pressure. The decrease in the oxidation
    rate constants with increasing pressure is considered to result from the reduction
    in voids in the formed oxide scales, which decreases the contact area between
    dissolved oxygen in steam or supercritical water and the metal.
  description_type: abstract
  lang: und

## Creator

- name: Yoshiaki Toda
  role: author
  orcid: https://orcid.org/0000-0002-8343-2890
- name: Nina Kobata
  role: author
- name: Xianglan Li
  role: author
  orcid: https://orcid.org/0000-0003-0992-1722
- name: Masahiko Demura
  role: author
  orcid: https://orcid.org/0000-0002-7308-3041

## Contact agent



## Publisher

organization: The Iron and Steel Institute of Japan

## Managing organization



## Keyword

- subject: heat-resistant steel
  schema: not_defined
- subject: oxide scale
  schema: not_defined
- subject: oxidation rate constant
  schema: not_defined
- subject: oxidation reaction exponent
  schema: not_defined
- subject: pressure
  schema: not_defined
- subject: supercritical water
  schema: not_defined

## Rights

- identifier: https://creativecommons.org/licenses/by-nc-nd/4.0/

## Other identifier(s)



## Data origin

- data_origin_type: other

## Embargo



## Journal

- title: ISIJ International
  issn: '09151559'
  volume: '66'
  issue: '12'
  article_number: ISIJINT-2026-179

## Conference



## Related item



## Funding

- identifier: 25K08550
  funder_name: JSPS
  description: Grand-in-Aid for Scientific Research (C) "Oxidation and Corrosion Behavior
    of Metallic Materials by Acidic Supercritical Water Mixed with Solid Particles"
- funder_name: The Iron and Steel Institute of Japan
  description: ISIJ Research Promotion Grant "Oxidation and Corrosion Behavior of
    Heat-resistant Steels in Simulated Geothermal Fluids with High Temperature, Pressure,
    and Acidity"

## Instrument



## Instrument operator



## Instrument managing organization



## Measurement method



## Specimen



## Chemical composition



## Structure for specimen



## Structural feature for specimen



## Specific property for specimen



## Process for specimen treatment



## Computational method



## Energy level/transition state



## Software



## Custom property



## Fileset

- id: 9563e6fb-f5f1-4eab-9cec-a923bf1f20e7
  filename: 20267Toda-ISIJInt.pdf
  content_type: application/pdf
  size: 3024053
  md5: 7e742804e0eb7a4fed9f5f4bf9794b4a

## Thumbnail

fileset_id: 9563e6fb-f5f1-4eab-9cec-a923bf1f20e7
filename: 20267Toda-ISIJInt.pdf