説明:
(abstract)9Cr ferritic/martensitic heat-resistant steel and 18Cr austenitic steel were exposed for various durations in a pressure vessel to steam (0.5 MPa), subcritical water (10.2 MPa), and supercritical water (22.7 MPa) at 650 °C. The pressure dependence of the oxidation rate constants of each material was determined from the time dependence of specimen weight gain and oxide scale thickness due to oxidation. The oxidation rate constants of both steels decreased with increasing pressure. In steam, the oxidation rate constant of the 18Cr steel was smaller than that of the 9Cr steel. The difference between the two steels decreased with increasing pressure, and the oxidation rate constants of the two steels became almost identical in supercritical water. These results suggest that, at 650 °C, boilers and pressure vessels can be safely operated using higher-pressure steam or supercritical water at the same temperature if they are designed based on the oxidation behavior of heat-resistant steels in steam at atmospheric pressure. The decrease in the oxidation rate constants with increasing pressure is considered to result from the reduction in voids in the formed oxide scales, which decreases the contact area between dissolved oxygen in steam or supercritical water and the metal.
権利情報:
キーワード: heat-resistant steel, oxide scale, oxidation rate constant, oxidation reaction exponent, pressure, supercritical water
刊行年月日: 2026-11-15
出版者: The Iron and Steel Institute of Japan
掲載誌:
研究助成金:
原稿種別: 出版者版 (Version of record)
MDR DOI:
公開URL: https://doi.org/10.2355/isijinternational.isijint-2026-179
関連資料:
その他の識別子:
連絡先:
更新時刻: 2026-11-16 11:51:45 +0900
MDRでの公開時刻: 2026-11-17 18:29:01 +0900
| ファイル名 | サイズ | |||
|---|---|---|---|---|
| ファイル名 |
20267Toda-ISIJInt.pdf
(サムネイル)
application/pdf |
サイズ | 2.88MB | 詳細 |