# チタン合金のギガサイクル疲労における 微小内部き裂の非破壊観察

https://mdr.nims.go.jp/datasets/584f5334-e657-4856-ae02-9d979667303e

## File

- [770_チタン合金のギガサイクル疲労における微小内部き裂の非破壊観察 (1).pdf](https://mdr.nims.go.jp/filesets/91a6171a-c0f3-4b9d-a01f-9233ea703610/download) ([Detail](https://mdr.nims.go.jp/filesets/91a6171a-c0f3-4b9d-a01f-9233ea703610.md))

## Id

584f5334-e657-4856-ae02-9d979667303e

## Local identifier



## Visibility

open_to_public

## State

published

## Created at

2025-01-09T01:13:20.201849Z

## Updated at

2025-11-01T23:30:06.529639Z

## Published at

2025-11-01T23:22:09.056315Z

## Doi



## First published url

https://doi.org/10.2320/materia.63.770

## Date published

2024-11-01

## Recorded date published

2024

## Resource type

journal_article

## Manuscript type

vor

## Collection



## Title

- title: チタン合金のギガサイクル疲労における 微小内部き裂の非破壊観察
  title_type: original
  lang: ja

## Description

- description: 鋼材のS-N 曲線は，一般に10^6～10^7 回程度の繰返し領域で水平部，すなわち疲労限度を示す．しかし，この疲労限度以下の応力でも，10^7
    回を超える領域において，材料内部を起点として疲労破壊を生じる挙動(内部破壊)が認識されるようになった．この現象は，超高サイクル疲労やギガサイクル疲労と呼ばれ，1980年代にその存在が確認されて以来，国内外で活発な研究が進められてきた．しかしながら内部破壊の本質的なメカニズムが明らかにされたとは言い難い．本報告では、マルチスケールX
    線CT とその場疲労試験を用いた非破壊観察手法を紹介し，これを2 種類のチタン合金((α＋β)型Ti-6Al-4V およびβ型Ti-22V-4Al)に適用することで，ギガサイクル疲労における内部き裂の発生・進展挙動と合金種の関連について検討する．
  description_type: abstract
  lang: und

## Creator

- name: 中村 孝
  role: author
- name: 吉中 奎貴
  role: author
  orcid: https://orcid.org/0000-0003-0534-7815
  organization: National Institute for Materials Science
  ror: https://ror.org/026v1ze26
- name: 薛 高格
  role: author
- name: 藤村 奈央
  role: author
- name: 髙橋 航圭
  role: author

## Contact agent



## Publisher

organization: 公益社団法人 日本金属学会

## Managing organization



## Keyword

- subject: 疲労
  schema: not_defined
- subject: き裂
  schema: not_defined
- subject: 放射光
  schema: not_defined
- subject: 非破壊観察
  schema: not_defined

## Rights

- identifier: http://rightsstatements.org/vocab/InC/1.0/

## Other identifier(s)



## Data origin

- data_origin_type: other

## Embargo

start_date: 2024-11-01
end_date: 2025-11-01

## Journal

- title: まてりあ
  volume: '63'
  issue: '11'
  start_page: 770
  end_page: 775

## Conference



## Related item



## Funding



## Instrument



## Instrument operator



## Instrument managing organization



## Measurement method



## Specimen



## Chemical composition



## Structure for specimen



## Structural feature for specimen



## Specific property for specimen



## Process for specimen treatment



## Computational method



## Energy level/transition state



## Software



## Custom property



## Fileset

- id: 91a6171a-c0f3-4b9d-a01f-9233ea703610
  filename: 770_チタン合金のギガサイクル疲労における微小内部き裂の非破壊観察 (1).pdf
  content_type: application/pdf
  size: 928408
  md5: 27fb1883276c1ac4d50d4f8350f8929f

## Thumbnail

fileset_id: 91a6171a-c0f3-4b9d-a01f-9233ea703610
filename: 770_チタン合金のギガサイクル疲労における微小内部き裂の非破壊観察 (1).pdf