Original data for Fig.2.6(c), Unstable, in a NIMS Monograph titled "fiber fuse"
1 of 16
Original data for Fig.2.6(c), Unimodal mode, in a NIMS Monograph titled "fiber fuse"
2 of 16
Original data for Fig.2.6(c), 3.1(a) and 3.4; Cylindorical mode, in a NIMS Monograph titled "fiber fuse"
3 of 16
Original data for Fig.2.6(a) and (b), Unstable mode, in a NIMS Monograph titled "fiber fuse"
4 of 16
Original data for Fig.2.6(a) and (b), Unimodal mode, in a NIMS Monograph titled "fiber fuse"
5 of 16
Original data for Fig.2.6(a) and (b), Cylindorical mode, in a NIMS Monograph titled "fiber fuse"
6 of 16
Original data for Fig.3.8(a) and (b), bare fibers, in a NIMS Monograph titled "fiber fuse" , Part 2/2
7 of 16
Original data for Fig.3.8(a), bare fibers immersed in water, in a NIMS Monograph titled "fiber fuse"
8 of 16
Original data for Fig.3.8(a), acrylate coated fibers, in a NIMS Monograph titled "fiber fuse"
9 of 16
Original data for Fig.3.8(a) and (b), bare fibers, in a NIMS Monograph titled "fiber fuse" , Part 1/2
10 of 16
Original data for Fig.3.8(a), acrylate coated fibers, in a NIMS Monograph titled "fiber fuse"
11 of 16
Original data for Fig.3.8(b), bare fibers, in a NIMS Monograph titled "fiber fuse"
12 of 16
Original data for Fig.3.9, acrylate coated fibers, in a NIMS Monograph titled "fiber fuse"
13 of 16
Original data for Fig.3.9, bare fibers, in a NIMS Monograph titled "fiber fuse"
14 of 16
Fiber fuse damage in the optical fibers called LEAF, Corning
15 of 16
Fiber fuse damage in the optical fibers called TrueWave RS, OFS